供應(yīng)抗紫外線(xiàn)POM 日本三菱 F20-54 耐老化POM
操作 | 牌號(hào) | 熔融體積流量(MVR) (cm3/10min) | 簡(jiǎn)支梁缺口沖擊強(qiáng)度 (kJ/m2) | 抗張強(qiáng)度 (MPa) | 拉伸斷裂應(yīng)變 (%) | 表面電阻率 (ohms) |
A10-03 | 2.2 (190°C/2.16 kg) | 8.0 (23°C) | 67.0 (屈服, ISO 527-1, -2) | 35 (50 mm/min) | 1.0E+16 | |
A25-03 | 12 (190°C/2.16 kg) | 8.0 (23°C) | 69.0 (屈服, ISO 527-1, -2) | 35 (50 mm/min) | 1.0E+16 | |
F10-01 | 2.2 (190°C/2.16 kg) | 8.0 (23°C) | 63.0 (屈服, ISO 527-1, -2) | 33 (50 mm/min) | 1.0E+16 | |
F10-02 | 2.2 (190°C/2.16 kg) | 8.0 (23°C) | 63.0 (屈服, ISO 527-1, -2) | 33 (50 mm/min) | 1.0E+16 | |
F10-EW | 3.4 (190°C/2.16 kg) | 8.0 (23°C) | 62.0 (屈服, ISO 527-1, -2) | 35 (50 mm/min) | ||
F20-03 | 7.7 (190°C/2.16 kg) | 7.0 (23°C) | 64.0 (屈服, ISO 527-1, -2) | 30 (50 mm/min) | 1.0E+16 | |
F20-05 | 7.7 (190°C/2.16 kg) | 7.0 (23°C) | 64.0 (屈服, ISO 527-1, -2) | 30 (50 mm/min) | 1.0E+16 | |
F20-54 | 7.7 (190°C/2.16 kg) | 6.5 (23°C) | 62.0 (屈服, ISO 527-1, -2) | 30 (50 mm/min) | 1.0E+16 | |
F20-61 | 7.7 (190°C/2.16 kg) | 6.0 (23°C) | 63.0 (屈服, ISO 527-1, -2) | 30 (50 mm/min) | 1.0E+13 | |
F20-EW | 7.7 (190°C/2.16 kg) | 7.0 (23°C) | 64.0 (屈服, ISO 527-1, -2) | 30 (50 mm/min) | ||
F25-03 | 14 (190°C/2.16 kg) | 6.5 (23°C) | 64.0 (屈服, ISO 527-1, -2) | 27 (50 mm/min) | 1.0E+16 | |
F30-03 | 23 (190°C/2.16 kg) | 6.0 (23°C) | 64.0 (屈服, ISO 527-1, -2) | 25 (50 mm/min) | 1.0E+16 | |
F30-05 | 23 (190°C/2.16 kg) | 6.0 (23°C) | 64.0 (屈服, ISO 527-1, -2) | 25 (50 mm/min) | 1.0E+16 | |
F40-03 | 45 (190°C/2.16 kg) | 5.0 (23°C) | 64.0 (屈服, ISO 527-1, -2) | 20 (50 mm/min) | 1.0E+16 | |
FRC-20 | 8.3 (190°C/2.16 kg) | 8.0 (23°C) | 57.0 (屈服, ISO 527-1, -2) | 42 (50 mm/min) | ||
FV-30 | 27 (190°C/2.16 kg) | 6.0 (23°C) | 63.0 (屈服, ISO 527-1, -2) | 30 (50 mm/min) | 1.0E+13 |