PC IRY2200 日本出光石油化學(xué)株式會(huì)社 物性數(shù)據(jù) |
①原料描述部分 |
|||
規(guī)格級(jí)別: |
阻燃級(jí) |
外觀顏色: |
--- |
備注說(shuō)明: |
特性:低粘度、防火等級(jí)新V-0 |
②原料技術(shù)數(shù)據(jù) |
|||||
性能項(xiàng)目 |
試驗(yàn)條件[狀態(tài)] |
測(cè)試方法 |
測(cè)試數(shù)據(jù) |
數(shù)據(jù)單位 |
|
基本性能 |
吸水率 |
--- |
--- |
0.23 |
% |
熔體流動(dòng)速率 |
--- |
--- |
12 |
g/10min |
|
物理性能 |
光線透射率 |
--- |
--- |
85~89 |
% |
比重 |
--- |
--- |
1.20 |
--- |
|
機(jī)械性能 |
伸張屈服強(qiáng)度 |
--- |
--- |
64 |
MPa |
伸張抗斷強(qiáng)度 |
--- |
--- |
68 |
MPa |
|
伸張彈性模量 |
--- |
--- |
2300 |
MPa |
|
破壞伸張率 |
--- |
--- |
115 |
% |
|
抗撓強(qiáng)度 |
--- |
--- |
93 |
MPa |
|
彎曲彈性模量 |
--- |
--- |
2350 |
MPa |
|
IZOD沖擊強(qiáng)度 |
4mm |
--- |
70 |
KJ/m2 |
|
IZOD沖擊強(qiáng)度 |
3.2mm |
--- |
90 |
KJ/m2 |
|
羅氏硬度 |
--- |
--- |
R120(M75) |
--- |
|
滑動(dòng)摩擦 |
--- |
--- |
12 |
--- |
|
電氣性能 |
絕緣破壞電壓 |
--- |
--- |
30 |
kv/mm |
體積固有電阻 |
--- |
--- |
<1016 |
Ω.m |
|
電容率 |
60Hz |
--- |
2.91 |
--- |
|
電容率 |
1MHz |
--- |
2.85 |
--- |
|
介質(zhì)衰耗因數(shù) |
60Hz |
--- |
6.6×10-4 |
--- |
|
介質(zhì)衰耗因數(shù) |
1MHz |
--- |
9.2×10-4 |
--- |
|
耐電弧性 |
--- |
--- |
110 |
sec |
|
加工性能 |
成型收縮率 |
--- |
--- |
0.5~0.7% |
% |
熱 性 能 |
線膨脹系數(shù) |
--- |
--- |
6.5 |
×10-5cm/cm/℃ |
燃燒性 |
3mm |
--- |
V-0 |
--- |
|
載荷撓曲溫度 |
--- |
--- |
148 |
℃ |
|
維卡軟化點(diǎn) |
--- |
--- |
148 |
℃ |